Product Overview
A zirconia ceramic rod is used where a ceramic part has to take impact, wear, or bending load that an alumina rod cannot survive. It is installed in pump shafts and valve parts, as grinding media and grinding rods, in precision structural and wear parts, and in medical and dental applications. The material is selected for toughness and strength, not for insulation.
Strength and Toughness Data
|
Item |
Value |
|
Material |
Yttria-stabilized zirconia (Y-TZP) |
|
Flexural strength |
900–1200 MPa |
|
Fracture toughness |
6–15 MPa·m¹/² |
|
Hardness |
1200–1400 HV |
|
Maximum operating temperature |
≤ 1000°C (long-term) |
|
Diameter |
3–100 mm |
|
Length |
10–500 mm |
|
Surface |
Precision ground / polished |
Flexural strength of 900–1200 MPa and fracture toughness of 6–15 MPa·m¹/² are well above alumina. This is what allows the rod to be used in positions where impact or bending load would crack an alumina part.
Phase Transformation Toughening
When zirconia is loaded, the tetragonal phase transforms to the monoclinic phase. This transformation absorbs energy and stops cracks from propagating, which is the mechanism behind the higher toughness compared with alumina. The effect is what makes the material suitable for wear and impact applications.
Temperature Limit
The phase transformation toughening effect decreases at high temperature, so long-term service is recommended below 1000°C. Above that, the toughness advantage narrows. If the application runs hot, the working temperature should be stated so the material choice can be assessed.
Applications
Pump shafts and valve parts
01
Grinding media and grinding rods
02
Precision structural and wear parts
03
Medical and dental components
04
FAQ
Q: How do I choose between a zirconia and an alumina rod?
A: If the application requires toughness, wear resistance, or impact resistance, zirconia is the correct choice. If the requirement is mainly insulation and cost matters, alumina is the lower-cost option.
Q: Does zirconia lose toughness at high temperature?
A: The phase transformation toughening effect decreases at high temperature, so long-term service is recommended below 1000°C. Provide the working temperature so the material choice can be assessed.
Hot Tags: zirconia ceramic rod, China zirconia ceramic rod manufacturers, suppliers, factory, Ceramic Fiber Tube, Ceramic Parts, industrial ceramics, Macor Tube, Mullite Ceramic Tubes, Silicon Carbide Tubes